ref | title | DOI | material type | comment |
---|---|---|---|---|
383 | Advancement of capture immunoassay for real-time monitoring of hepatitis E virus-infected monkey | https://doi.org/10.1016/j.aca.2020.02.020 | Metal | AuNPs@Ag |
ref | material | size | size err | size unit | size type | size comment | BET | b nanozyme | b 10n | b unit | specific act | sa 10n | sa unit | comment |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
383 | AuNPs@Ag | 24.4 | nm | DLS | The hydrodynamic size of AuNPs were found 13.66 ± 3.66 nm with polydispersity index of 0.273 which increased to 24.4 nm after the Ag deposition, measured by DLS |