ref | material | size | size err | size unit | size type | size comment | BET | b nanozyme | b 10n | b unit | specific act | sa 10n | sa unit | comment | |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
7943 | 734 | ZrO2 NPs | The individual ZrO2 NP has a size range from 20 nm to 40 nm, and slight aggregation of the particles can be observed from the TEM images. Fig. 1B shows the dynamic light scattering spectra of the ZrO2 NPs, the hydrodynamic diameters of ZrO2 NPs were in the range from 90 nm to 200 nm, which confirms the slight aggregation. |
ref | material | enzyme type | substrate | pH | T | km | km err | km 10n | km unit | vmax | vmax err | vmax 10n | vmax unit | kcat | kcat err | kcat 10n | kcat unit | kcat/km | kcat/km 10n | kcat/km unit | comment | |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
6642 | 734 | ZrO2 NPs | hydrolase | 4-MUP | 14.7 | μM | 5.31 | -9 | M/s | 2.74 | 1/s | 734 | 6 | M-1 s-1 |
ref | material | application | target | method | linear range | linear ran unit | LOD | lod unit | recovery | comment | |
---|---|---|---|---|---|---|---|---|---|---|---|
5657 | 734 | ZrO2 NPs | near-infrared intracellular imaging |
ref | title | DOI | material type | comment | |
---|---|---|---|---|---|
3920 | 734 | The phosphatase-like activity of zirconium oxide nanoparticles and their application in near-infrared intracellular imaging | https://doi.org/10.1039/D0TB00450B | Metal oxide | zirconium oxide nanoparticles (ZrO2 NPs) |