ref | title | DOI | material type | comment | |
---|---|---|---|---|---|
3766 | 579 | Effects of crystal structure on the activity of MnO 2 nanorods oxidase mimics | https://doi.org/10.1007/s12274-020-2680-5 | Metal oxide | MnO2 nanorods |
ref | material | size | size err | size unit | size type | size comment | BET | b nanozyme | b 10n | b unit | specific act | sa 10n | sa unit | comment | |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
7807 | 579 | MnO2 | μm | TEM, SEM | Figure 2 shows that all of the MnO2 samples were assembled to form the same morphology, nanorods. α-MnO2 nanorods were 15–95 nm in diameter and 0.27–1.3 μm in length. β-MnO2 nanorods were 40–130 nm in diameter and 0.64–2.78 μm in length. γ-MnO 2 nanorods were 18–105 nm in diameter and 0.2–0.7 μm in length. | 33.700000000000003 |
ref | material | enzyme type | substrate | pH | T | km | km err | km 10n | km unit | vmax | vmax err | vmax 10n | vmax unit | kcat | kcat err | kcat 10n | kcat unit | kcat/km | kcat/km 10n | kcat/km unit | comment | |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
6461 | 579 | MnO2 | OXD | TMB | 3.45 | μM | 16.80 | -6 | M/s | 579 | 579 |
ref | material | application | target | method | linear range | linear ran unit | LOD | lod unit | recovery | comment | |
---|---|---|---|---|---|---|---|---|---|---|---|
5518 | 579 | MnO2 | Detection of glutathione | glutathione | colorimetric | 0.11-45 | μM | 0.1 | μM |